Zinc can be coated on iron to produce galvanized iron but the reverse is not possible. It is because
- Azinc is lighter than iron
- Bzinc has lower melting point than iron
- Czinc has lower negative electrode potential than iron
- Dzinc has higher negative electrode potential than iron
View written solutionFree
Correct answer: D
The reduction potential values are
E°Zn2+/Zn = – 0.76 V
E°Fe2+/Fe = – 0.44 V
Thus, due to higher negative electro potential value
of zinc than iron, iron cannot be coated on zinc.
More from Electrochemistry
- The number of electrons delivered at the cathode during electrolysis by a current of 1 ampere in 60 seconds is (charge on electron = 1.60 1019C)2016 · MCQ
- Aqueous solution of which of the following compounds is the best conductor of electric current ?2015 · MCQ
- A device that converts energy of combustion of fuels like hydrogen and methane, directly into electrical energy is known as2015 · MCQ
- The weight of silver (at. wt. = 108) displaced by a quantity of electricity which displaces 5600 mL of O2 at STP will be2014 · MCQ
- When 0.1 mol MnO is oxidised the quantity of electricity required to completely oxidise MnO to MnO is2014 · MCQ
- Consider the half-cell reduction reaction Mn2+ + 2e Mn, Eo = 1.18 V Mn2+ Mn3+ + e, Eo = 1.51 V The o for the reaction 3 Mn2+ Mno + 2Mn3+, and possibility of the forward reaction are respectively2013 · MCQ
- How many gram of cobalt metal will be deposited when a solution of cobalt (II) chloride is electrolyzed with a current of 10 amperes for 109 minutes (1 Faraday = 96,500 C; Atomic mass of Co = 59 u)2013 · MCQ
- At 25oC molar conductance of 0.1 molar aqueous solution of ammonium hydroxide is 9.54 ohm1 cm2 mol1 and at infinite dilution its molar conductance is 238 ohm1 cm2 mol1. The degree of ionisation of ammonium hydroxide at the same…2013 · MCQ